Please download our PDF for detailed technical data.
property | value | unit | tolerance |
total thickness | 100 | µm | ± 4µm |
density | 0,906 | g/cm³ | |
melt flow rate (230°C and 2,16 kg) | 13,0 | g/10 min. | |
puncture resistance | 29,3 | N | |
unit weight | 92,8 | g/m² | ± 0,5g/m² |
yield | 10,77 | m²/kg | ± 0,03m²/kg |
dimensional stability | |||
machine direction MD | -2,4 | % | ± 0,5% |
transverse direction TD | 1,2 | % | ± 0,3% |
bond strength | 6,9 | N/15 mm | |
tensile strength | |||
machine direction MD | 156 | N/mm² | |
transverse direction TD | 148 | N/mm² | |
machine direction MD (-25°C) | 198 | N/mm² | |
breaking elongation | |||
machine direction MD | 54 | % | |
transverse direction TD | 76 | % | |
machine direction MD (-25°C) | 37 | % | |
gloss | > 100 | % | |
haze | 2,4 | % | |
transparency | 91,8 | % | ± 0,1% |
oxygen transmission rate | |||
(23° C/50% RH) | 440 | cm³/(m²*d*bar) | |
(38° C/0% RH) | 960 | cm³/(m²*d*bar) | |
water vapour transmission rate | |||
(23°C, 85%/0% RH) | 0,30 | g/(m²*d) | |
(38°C, 90%/0% RH) | 1,49 | g/(m²*d) | |
treatment level | 38 | dyn |